How to prevent the blocking of Release Liners during storage?

Hey there, it’s [Your Company Name] – your go-to release liner supplier, and we’ve heard it all: “Why are my liners sticking together during storage?” “I opened a box I stored for 3 months, and half of them are useless.” If that’s you, you’re not alone. Blocking (that annoying case where adhesive-coated release liners glue themselves shut, or liner layers stick to each other) is one of the most common headaches we get from converting companies, label manufacturers, and even big packaging brands. The good news? Most of the time, it’s totally preventable – no fancy, expensive fixes required. Let’s break this down like we do with our clients, no stuffy jargon, just real stuff that works. Release Liner

First, let’s keep it basic: what actually causes release liner blocking? It’s not just “bad liners” – it’s usually a mix of three things: the liner itself, the adhesive on whatever’s attached to it, and how you store the rolls or sheets. Let’s start with the liner specs, because that’s our wheelhouse. Here’s the deal: not all release liners are made equal. The silicone coating (the “release layer” that makes the liner slippery for adhesive) is the star here. If the silicone is too thin, or cured wrong, it doesn’t bond properly to the liner base (usually paper, PET, or PP). Over time, that weak silicone can transfer to the adhesive on the opposite side of the liner – and that’s when sticking happens. We see this a lot with customers who buy cheap, off-brand liners to save a buck; 9 times out of 10, that’s the root cause. Our liners, by contrast, use a calibrated silicone coat – we test every batch to make sure the release force is consistent, not too loose (which causes transfer) and not so tight it ruins your processing. Pro tip: ask your supplier for the silicone coat weight and release force specs. If they can’t give you that, walk away – it’s a red flag.

Then there’s the adhesive side. Wait, you might be thinking, blocking is on the liner side – but nope, the adhesive plays a huge role. If your product’s adhesive is too aggressive (like some hot-melt or acrylic adhesives used for shipping labels), it will seep into the liner’s silicone layer if there’s any gap. That’s called “adhesive bleed-through.” How does storage tie into this? If you’re stacking liner sheets flat, or winding rolls too tight, the pressure squeezes that adhesive into the silicone. For rolls, the tension you use when winding is critical. We’ve had clients wind their rolls so tight they could barely bend ’em – and after a month in a warm warehouse, they were glued solid. Our advice? When you’re winding your finished rolls (after we ship them), stick to the recommended tension for your adhesive: 10-15 psi for most label applications, 5-10 psi for thinner liners like our 1.5 mil PET. And don’t wind them so tight that the core indents – that’s a quick way to set the adhesive into the liner.

Now, the part most people overlook: storage conditions. This is where 80% of blocking happens, and it’s totally in your control. Let’s talk temperature and humidity first. Silicone and adhesive don’t like extreme heat or cold. If you store liners in a warehouse that hits 90°F (32°C) in the summer, the silicone breaks down, and the adhesive gets way stickier – basically, they want to bond. Cold isn’t great either: if your liners are frozen and then thawed, the silicone can crack, leading to transfer. Humidity’s a big one too. Paper liners, in particular, absorb moisture if stored in a damp space. Wet paper swells, and the adhesive can stick to the swollen surface – even the best silicone won’t hold up. We recommend storage temps between 60-75°F (15-24°C) and relative humidity 40-55%. If your warehouse is way off that, invest in a small dehumidifier or space heater for the liner storage area – it’s way cheaper than replacing a whole batch of blocked liners.

Then there’s how you organize the storage. Let’s start with rolls, since that’s how most of our customers get them. Don’t stand rolls on their ends unless you have to – standing a roll on its side for weeks puts constant pressure on the outermost layers, which can squeeze adhesive or silicone. The best way is to store rolls horizontally, stacked no more than 3-4 high. Stacking more than that squishes the bottom rolls, and the weight pushes the layers together – blocking gold, basically. For sheets, don’t stack them flat on the floor or against a wall. Lift ’em onto shelves, so air can circulate around each stack. If you have to stack sheets, keep the stack height under 12 inches, and place a piece of corrugated cardboard between every 5 sheets to add a little space and reduce pressure. We’ve had a client who stored 20 stacks of sheets on the floor in a damp basement – half blocked in 2 weeks. We moved ’em to pallets on shelves with dehumidifiers, and they were good for 3 months. That’s a $1,000 mistake fixed with a $200 fix.

Another big one: what you store liners next to. Duh, don’t store liners with chemicals or solvents – those fumes can break down the silicone layer, making it sticky. We’ve had a customer who kept a case of cleaning supplies next to his liner rolls – the fumes got into the liners, and when he opened a roll, the whole outer layer was gluey. Also, avoid storing liners near heavy machinery that vibrates – vibration can loosen the silicone, leading to transfer. And for the love of all things adhesive, don’t tape boxes of liners shut with strong packing tape directly on the liners – the adhesive from the tape can transfer, causing blocking on the exposed surfaces.

Wait, what about if you’re storing liners that are already coated? Let’s say you’re a converter who has a lot of coated liners waiting to be processed. We get this a lot. If you’re not using them within 2 weeks, here’s a quick hack: wrap the rolls or sheets in poly bags that are semi-permeable – not airtight, not super loose. Airtight bags trap moisture, which is bad, and loose bags let too much humidity in. Semi-permeable ones (we can even supply these if you’re low) keep the humidity stable. Label the bags with the date you received them – first in, first out! Don’t grab a 3-month-old roll to use before a 1-week-old one. Older liners are way more prone to blocking, so rotating your stock is non-negotiable. We’ve had clients throw away “new” rolls because they grabbed the oldest ones first and they blocked – simple inventory fix, no extra cost.

Let’s talk about common mistakes we see all the time, just to make sure you don’t do ’em. First, “we stored them in a climate-controlled office, so it’s fine!” No – offices have different humidity than warehouses. Offices are dry in the winter (heaters running) which can make paper liners brittle, and damp in the summer (AC running) which is bad for both paper and silicone. Second, “we never had blocking before, so why now?” Silicone batches can vary slightly if the supplier cuts corners, but more likely, you changed your adhesive, or moved your warehouse, or the summer hit harder than last year. Don’t assume it’s “just how it is” – test a small batch first when you get new liners, before you store the whole pallet. Cut a 6-inch piece from the outer layer, another from the inner core, press ’em together for 24 hours at room temp, peel ’em apart. If they stick, you know you have a problem before it’s 1,000 lbs of blocked liners.

And hey, if you’re dealing with blocked liners already, it’s not always a lost cause. If it’s just the outer layer of a roll, you can unroll the outer 10-15 feet, and the inner layers will usually be fine. For sheets, if it’s just the edges, trim ½ inch off each side and they’re ready to go. But if the whole batch is solid, don’t risk running it through your press – it’ll gum up your blades, waste more time and money than replacing the liners.

Here’s the thing: as a release liner supplier, our job isn’t just to ship you liners – it’s to help you avoid headaches like blocking. We work with all kinds of clients, from small label shops to big consumer goods brands, and we’ve seen every blocking scenario you can think of. If you’re having issues, don’t guess – reach out, and we’ll walk you through your storage setup, your liner specs, and your processing. We can even send a free sample of our premium release liners, with their release force and silicone coat weight specs, to test against what you’re using now.

BOPP Film If you’ve tried all the tricks and you’re still dealing with blocking, or if you want to switch to liners that are made to hold up during storage, we’re here to help. Hit us up to chat, no sales pitch, just straight talk about what’ll work for your operation.

References

  1. “Release Liner Technology and Applications,” TAPPI Press, 2021.
  2. Adhesive Transfer and Blocking in Pressure-Sensitive Products, Pressure Sensitive Tape Council (PSTC) Technical Bulletin 17, 2020.
  3. Warehouse Storage Best Practices for Flexible Packaging Materials, Flexible Packaging Association (FPA) White Paper, 2022.

Hangzhou Weshare Import & Export Co., Ltd.
As one of the most professional release liner manufacturers and suppliers in China, we’re featured by quality products and good service. Please rest assured to wholesale customized release liner made in China here from our factory. Contact us for free sample.
Address: Room B-308, XingShang Development Building, No.1243 MoGanShan Rd, HangZhou, China
E-mail: grace@weshare-china.com
WebSite: https://www.weshareprint.com/